2018 Jeep Wrangler JL frame defect may force sales stoppage, recall

Add as a preferred source on Google

Fiat Chrysler Automobiles’ (FCA) new generation Jeep Wrangler JL has a problem. Certain Wrangler JLs have defective frame welds that can result in the popular SUV’s track bar separating from the frame, causing immediate steering problems and potential crashes, Japolnik reported.

It is not yet clear which model Wrangler JLs or how many vehicles are affected by the recall, because to date FCA has not made a public statement. We’ll cycle back to update this article with more specifics as news develops.

Recommended Videos

In an update on the JL Wrangler’s forum on Friday, October 5, 2018, a member with the profile name “Lablue” wrote, “FCA has started the recall UA5 for the track bar weld issue. This affects about 18,000 JL Wranglers. The issue exists on about 4 percent of the recalled vehicles, says FCA. Some of the defective JL’s haven’t been sold yet, FCA ordered dealers to halt sales of the recalled Wranglers until vehicles are inspected and repaired, if needed.”

Lablue also posted what he claims is an FCA Safety Recall Advanced Communication about a 2018 through 2019 JL Jeep Wrangler safety recall and stop-sale order for vehicles included in the recall.

Under the Reason for This Safety Recall subhead, the official-looking document states: “Some of the above vehicles may have been built with a front track bar bracket weld located off the seam potentially resulting in the bracket separating from the frame. The separation of the front track bar bracket from the frame may cause a reduction in the steering response, which can cause a vehicle crash without prior warning.”


Japolnik reported that an FCA spokesperson confirmed “recall notices are pending” regarding track bar bracket weld failures.

The National Highway Traffic Safety Administration (NHTSA) has not issued a recall for the 2018 Wrangler JL regarding frame welds. However, searching the NHTSA site for complaints about the 2018 Wrangler JL finds 133 complaints about steering and 13 complaints about structure.

If you have  2018 Wrangler JL you can check whether your vehicle is part of the recall at the Mopar Recalls Search site. You will need the Vehicle Identification Number (VIN) to determine if your Jeep is affected. Because this situation is still developing, even if you check today and you do not see a recall for your VIN, it would be a good idea to check again in a few days after FCA issues an expected public statement.

Bruce Brown
Bruce Brown Contributing Editor   As a Contributing Editor to the Auto teams at Digital Trends and TheManual.com, Bruce…
Waymo’s robotaxis keep finding new things to drive into, and construction zones are the latest
Thirteen construction zone incidents, one fleet recall, and a passenger who thought the end was near.
A Hyundai Ioniq 5 is equipped as a robotaxi.

Waymo has recalled its entire fleet of nearly 4,000 robotaxis to prevent them from driving on highways after identifying at least 13 instances where its vehicles drove straight into highway sections closed for construction. 

This is the company's sixth recall in under a year, and follows separate incidents involving flooded roads, telephone poles, chains and gates, towed trucks, and school buses.

Read more
BYD’s Great Tang eSUV offers 10-minute charging and a 590-mile range starting at $40,000
Spectacular specs, record preorders, and not a single one headed to America.
Car, Transportation, Vehicle

BYD just launched the Great Tang, a full-size electric SUV that offers the range of a regular gasoline-powered car and takes only slightly longer to refuel (read: recharge). 

The company's flagship eSUV starts at around $35,500 and gives most American electric SUVs a serious run for their money.

Read more
BMW is taking orders for the i3 way ahead of schedule, and it’s got a happy problem to blame
Too much demand, too good a car to make people wait until fall.
Bumper, Transportation, Vehicle

BMW planned to open order books for the new i3 sedan this fall, but now, the automaker is opening them this week instead. The reason is the kind of happy problem every automaker wishes they had.

As it turns out, too many people want to buy the car, and the automaker decided it would be rude to make them wait.

Read more